Abstract:
Objective&Method In order to promote the utilization of vanadium tailings, a vanadium tailing with high silicon content and low activity in Shangluo County was taken as the research object. By adding cement clinker and smelting slags to vanadium tailings, and through the new compound activator to effectively stimulate the chemical activity of raw materials, a vanadium tailing based cementing material with good performance was prepared. The cementation characteristics of the cementing material were analyzed by X-ray diffraction and scanning electron microscopy. Result The suitable mass ratio of vanadium tailings, smelting slags and cement clinker is 60∶15∶25, and the optimum dosage of compound activator XJJ01 is 5%. When the prepared cementing material and the whole tailings of vanadium tailings are used at the cement-sand ratio of 1∶8, the 3, 28 d compressive strengths of the prepared filling body test blocks are 0.42, 2.11 MPa, respectively, which meets the requirements of Z03 and H20 grades of cementing materials. At the action of XJJ01 activator, SiO
2, Al
2O
3 and CaO in vanadium tailings and smelting slags cooperate with water glass, calcium salt and reinforcing agent to form hydrated calcium silicate and ettringite, which is helpful to improve the overall chemical activity of cementing materials. Conclusion When the tailings are filled, the tailings particles are closely packed and cross-linked at the action of cementing materials to form a dense structure, which can ensure the strength of the filling body.