Abstract:
Objective The Savayarton gold deposit in Xinjiang has not been developed and utilized for a long time, and there are many kinds of harmful components. The gold grade is low, and the main gold-bearing minerals are pyrite and arsenopyrite. The distribution rate of natural gold is 22.23%, and the particle size of gold minerals is fine, less than 0.01 mm accounting for 96.97%. Method Flotation condition tests such as grinding fineness and reagent system were carried out on ore raw materials with Au content of 1.53 g/t, As content of 0.74% and C content of 1.34%. The dosage of activator was determined to be 100 g/t, and the composite collector was 2∶1. The open-circuit test of the whole process of two roughing was carried out. Result The gold grade of the flotation concentrate was 21.96 g/t, the recovery rate was 69.83%, and the cumulative distribution rate of middlings was 22.67%. The gold recovery rate of the whole process closed-circuit test was increased by 20.56%. The daily processing capacity of 0.92 t enlarged continuous test of ore dressing was carried out for 96 h. The flotation concentrate yield was 7.14%, the gold grade was 18.49 g/t, and the recovery rate was 89.32%. Conclusion The harmful components in the flotation concentrate were obviously enriched. The test can provide technical reference for the development and utilization of low-grade refractory gold resources.