CAO Huan, JIN Jianping, ZHAO Xiaoyi, et al. Low temperature sulfuric acid ripening-water leaching for vanadium extraction from stone coal vanadium ore[J]. Multipurpose Utilization of Mineral Resources, 2024, 45(3): 75-80. DOI: 10.3969/j.issn.1000-6532.2024.03.012
    Citation: CAO Huan, JIN Jianping, ZHAO Xiaoyi, et al. Low temperature sulfuric acid ripening-water leaching for vanadium extraction from stone coal vanadium ore[J]. Multipurpose Utilization of Mineral Resources, 2024, 45(3): 75-80. DOI: 10.3969/j.issn.1000-6532.2024.03.012

    Low Temperature Sulfuric Acid Ripening-water Leaching for Vanadium Extraction from Stone Coal Vanadium Ore

    • This is an article in the field of metallurgical engineering. The vanadium ore with vanadium containing sericite and illite in Shaanxi province was taken as the research object, low-temperature sulfuric acid ripening-water leaching process was used to extract vanadium. The effects of ripening temperature, ripening time, sulfuric acid dosage, sodium chloride dosage, leaching temperature, leaching time and liquid-solid ratio on vanadium leaching rate were investigated. The results show when 25% sulfuric acid and 0.8% sodium chloride are added to the stone coal vanadium ore, the sample is aged at 130 ℃ for 8 h, and the sample is leached at 55 ℃ for 2 h under the conditions of liquid-solid ratio of 1.5∶1, the vanadium leaching rate can reach more than 89%. This indicates that it is feasible to adopt low temperature sulfuric acid ripening and water leaching process to extract stone coal type vanadium ore.
    • loading

    Catalog

      /

      DownLoad:  Full-Size Img  PowerPoint
      Return
      Return