吴宁. 攀西某钒钛磁铁精矿浮选脱硫实验[J]. 矿产综合利用, 2022, 43(3): 126-131. DOI: 10.3969/j.issn.1000-6532.2022.03.022
    引用本文: 吴宁. 攀西某钒钛磁铁精矿浮选脱硫实验[J]. 矿产综合利用, 2022, 43(3): 126-131. DOI: 10.3969/j.issn.1000-6532.2022.03.022
    Wu Ning. Experimental Study on the Flotation Desulfurization of Vanadium Titanium Magnetite Concentrate in Panxi[J]. Multipurpose Utilization of Mineral Resources, 2022, 43(3): 126-131. DOI: 10.3969/j.issn.1000-6532.2022.03.022
    Citation: Wu Ning. Experimental Study on the Flotation Desulfurization of Vanadium Titanium Magnetite Concentrate in Panxi[J]. Multipurpose Utilization of Mineral Resources, 2022, 43(3): 126-131. DOI: 10.3969/j.issn.1000-6532.2022.03.022

    攀西某钒钛磁铁精矿浮选脱硫实验

    Experimental Study on the Flotation Desulfurization of Vanadium Titanium Magnetite Concentrate in Panxi

    • 摘要: 攀西某钒钛磁铁精矿中的TFe、TiO2和S的品位分别为53.75%、12.55%和0.76%,铁、钛主要以钒钛磁铁矿、钛铁矿的形式赋存,硫主要以磁黄铁矿的形式赋存。磁黄铁矿单体解离度低,富连生体多。为将该钒钛磁铁精矿中的硫脱除,采用浮选工艺进行了降硫实验研究。结果表明:采用一粗四精二扫浮选闭路流程,在以硫酸为pH值调整剂,丁黄+丁铵(5∶1)为捕收剂,2#油为起泡剂,粗选用量分别为2000 g/t、300 g/t、40 g/t,粗扫选得到的硫粗精矿再磨细度-38 μm 93.33%的条件下,可以获得S品位为28.65%,S回收率59.46%的硫精矿,TFe品位为53.79%,TFe回收率为98.51%,铁精矿S品位为0.29%的铁精矿。

       

      Abstract: Grades of Fe, TiO2 and S in the vanadium titanium magnetite concentrate in Panxi are 53.75%, 12.55% and 0.76%. Fe and Ti are mainly in the form of vanadium-titanium magnetite and ilmenite, while sulfur is mainly in the form of magnetic pyrite. In order to reduce the sulfur content of this vanadium titanium magnetite concentrate, a study on desulfurization was carried out by flotation. Results show that adopting the flotation closed circuit process with once roughing, four times cleaning and twice scavenging, the sulfur concentrate with S grade of 28.65% and S recovery of 59.46%, and iron concentrate with TFe grade of 53.79%, TFe recovery of 98.51%, S grade of 0.29 % can be obtained with the following conditions: sulfuric acid as pH regulator, butyl xanthate + ammonium butyrate (5:1) as collector, 2# oil as frother, of which the dosage were 2000 g/t, 300 g/t, 40 g/t in roughing and regrinding fineness of sulfide concentrate by roughing and scavenging was -38 μm content of 93.33 %.

       

    /